    I cut all my paint with gloss. I use a 50/50 ratio of whatever color and gloss. I heat all my heads, with the exception of my fiberguards heads, to where when I dip the head and tap the excess paint off it is glossy. I then dip the head immediately in water to cool. I bake all my heads at 220 degrees for 20 minutes. This includes my heads with 3D eyes and fiberguards heads. Once cool I then slap a coat of UV seal coat. No problems with drippy paint and my heads come on pretty swank. I also use a fluid bed and heat gun.

    Name:  F52DE95D-04A8-4CCB-9DAD-27E61714C808.jpg
Views: 534
Size:  90.4 KB
    Name:  A5CB1EC8-C532-4671-A602-E97E6933E726.jpg
Views: 593
Size:  61.1 KB
    Last edited by DrNip; 11-07-2017 at 06:29 AM.
    Likes Brimfisher LIKED above post

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  

BACK TO TOP