Probably comes from past experience of not doing enough prep work and having it redo things. Going down the lead pouring road, almost every site I used talked about fluxing, so I decided I would do it, took some time to process a 67 lb ingot, but it wasn't difficult.
I kind of equate it to soldering either Electonics or plumbing, doing the prep work makes the actually soldering part fairly simple. I also don't think I'll end up making enough jigs to use the 60+ pounds of pure lead and 50+ pounds of plumbers solder, I have. Probably do some bullet casting with it also.