
Originally Posted by
huntinslabs
Your pics look like your boat is aluminum. If it is I would go and get rid of the pressure treated wood asap. You will get a galvanic reaction and could ruin your hull. And it happens quick. Or at least put some of them teflon slicks or something to keep your boat from sitting directly on the bunks/carpet. The copper in the PT is what causes it and will saturate the carpet in no time.