Wish I had a video camera so I could tape doing the fluxing, it really does help.
fatman
Likes: 0
Thanks: 0
HaHa: 0
Well this could explain why every time I have poured lead it turned out pitted and hard. This is good to know for sure. Will have to make sure I remember when I pour this spring.
I love taking my kids fishing, now if I could just manage to fish at the same time.
Wish I had a video camera so I could tape doing the fluxing, it really does help.
fatman
I use candle wax. It works well and usually self ignites. One warning... the first time I dropped the wax in the pot and it burst into flames, I tried to blow it out. DO NOT DO THIS. Singed the eyebrows right off my fool head and caught some marabou on fire. Please use caution.
BEESWAX IS THE ONLY THING I USE. no problems
I put a peice of candle wax in there, along with a 6 inch peice of solder wire. I don't know which item caused the majic, but the jigheads are 100 percent smoother, pour better, and remain shiny for the longhaul. even with a cold mold, it's alot better.
The Do-it instruction booklet says that tin (solder) added will generally improve lead. Ditto "redear" on a long lasting shiny smooth finish. My preferred alloy is 4-5% tin by weight added to soft lead - more than that is a waste of expensive tin and too much tin can actually make an alloy harder to pour.