Made up a batch of clear baits with a colored core in them. I played around for a while trying to figure out the core shot but ran out of ideas. Is there a how to do a core shot on multi cavity moles anywhere? Or if anyone has a tip I would be interested. Here is what I came up in the mean time. I too am having issues withmy plastic browning very quickly. I am loading up the heat stabilizer and heating at 10 to 15 sec between each stir.